Chemical Composition
0.25 to 0.3
%    
97.1 to 97.8
%    (estimate)
1.3 to 1.6
%    
0.035
%  (maximum)  
0.03 to 0.05
%    
0.5 to 0.8
%    
0.08 to 0.13
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 