Chemical Composition
0.02 to 0.05
%    
0.18 to 0.24
%    
0.25
%  (maximum)  
98 to 99
%    (estimate)
0.8 to 1.1
%    
0.012
%  (maximum)  
0.035
%  (maximum)  
0.035
%  (maximum)  
0.25
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 