Chemical Composition
0.14 to 0.19
%    
0.8 to 1.1
%    
96.9 to 98
%    (estimate)
1 to 1.3
%    
0.035
%  (maximum)  
0.02 to 0.035
%    
0.4
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 