Chemical Composition
10.8 to 11.1
%    
84.4 to 85.2
%    (estimate)
4 to 4.5
%    
1.0 others
Cu is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
185
   
 
Other Information
Links



No warranty is given for the accuracy of these data