Chemical Composition
9.5 to 10.8
%    
85.5 to 88
%    (estimate)
2.5 to 3.75
%    
Cu is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
248
MPa    
20
% strain    
137
   
 
Other Information