Chemical Composition
0.15
%  (maximum)  
2
%    
97.5 to 97.7
%    (estimate)
0.35
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
248
MPa    
15
% strain    
 
Other Information