Chemical Composition
0.0025
%  (maximum)  
0.25
%    
0.6
%  (maximum)  
97.5 to 98.1
%    (estimate)
0.85
%    
0.15
%    
0.028
%    
0.65
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1210 to 1450
MPa    
1310 to 1690
MPa    
11
% strain    
360 to 500
   
 
Other Information
Plate: 190,000-245,000 TS; 175,000-210,000 YS; 11-16 El; 44-55 RA; 360-500 HB; For severe service applications, pressure vessels, wear plates. Heat treated, wear resistant plates.