Chemical Composition
0.22
%  (maximum)  
98.4 to 98.6
%    (estimate)
1.25
%    
0.015
%  (maximum)  
0.04
%    
0.05
%    
0.02
%  (minimum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
448
MPa    
15
% strain    
 
Other Information
Rolled: 80,000 TS minimum; 65,000 YS minimum; 15 El. For structures, buildings, bridges, derricks, mine cars, bus bodies. Structural plate, good weldability.
V 65 STEEL
 