Chemical Composition
0.15
%  (maximum)  
12 to 14
%    
85.8 to 88
%    (estimate)
0.07 S or Se min
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
552
MPa    
16
% strain    
185
   
 
Other Information
Soft: 75,000 TS; 35,000 YS; 14 El; 150 HB; 1/2 H-temper: 115,000 TS; 80,000 YS; 16 El; 185 HB; For valve trim, cold headed parts; corrosion resistant, free-cutting.
ALMET 416
 



No warranty is given for the accuracy of these data