Chemical Composition
98
%    (estimate)
1
%    
0.5
%    
0.5
%    
Al is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
234
MPa    
5
% strain    
 
Other Information