Chemical Composition
0.04
%  (maximum)  
22 to 24
%    
2.5 to 3.5
%    
39.2 to 46.6
%    (estimate)
0.75
%  (maximum)  
2.5 to 3
%    
26 to 28
%    
0.03
%  (maximum)  
0.015
%  (maximum)  
0.75
%  (maximum)  
0.4 to 0.7
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information