Chemical Composition
0.25 to 0.35
%    
0.75 to 1
%    
96.2 to 97.1
%    (estimate)
0.15 to 0.25
%    
1.75 to 2.25
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
552 to 1250
MPa    
689 to 1520
MPa    
2 to 22
% strain    
220 to 460
   
 
Other Information
Links
Organizations

 