Chemical Composition
0.025
%  (maximum)  
0.04 to 0.08
%    
0.05 to 0.1
%    
26 to 28
%    
36.5 to 42.3
%    (estimate)
1
%  (maximum)  
0.6 to 1
%    
31 to 33
%    
0.02
%  (maximum)  
0.01
%  (maximum)  
0.3
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information