Chemical Composition
0.08
%  (maximum)  
12 to 14
%    
85.9 to 88
%    (estimate)
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
420
MPa    
600 to 800
MPa    
20
% strain    
 
Other Information
Ferritic. Softened: 250 N/mm**2 YS, 400-600 N/mm**2 TS, 20 El. Hardened/tempered: 420 N/mm**2 YS, 600-800 N/mm**2 TS, 18 El. Strip. For mineral oil industry. WNr. 1.4000, EN 10099-2.
NIROSTA 4000
 