Chemical Composition
0.2
%  (maximum)  
24 to 26
%    
50.5 to 57.2
%    (estimate)
17 to 21
%    
1.8 to 2.3
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 