Chemical Composition
0.08
%  (maximum)  
18 to 20
%    
65.3 to 71.4
%    (estimate)
1 to 1.75
%    
0.9 to 1.1
%    
8 to 10
%    
0.75 to 1.75
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
156
   
 