Chemical Composition
0.002 to 0.006
%    
0.1 to 0.18
%    
0.4 to 0.8
%    
0.15 to 0.5
%    
95.8 to 97.6
%    (estimate)
0.6 to 1
%    
0.4 to 0.6
%    
0.7 to 1
%    
0.03 to 0.1
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
689
MPa    
786 to 931
MPa    
20 to 100
% strain    
 
Other Information
Heat treated: 114,000-135,000 TS; 100,000 YP min; 20.0 El min. For car and railroad bodies, agricultural equipment. High strength-low alloy constructional steel.