Chemical Composition
94 to 97.4
%    (estimate)
1 to 1.5
%    
0.1 to 0.3
%    
0.03 to 0.2
%    
1.5 to 4
%    
TC 3.5-3.75
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 