Chemical Composition
0.21
%  (maximum)  
0.35
%  (maximum)  
97.6 to 99.2
%    (estimate)
0.7 to 1.35
%    
0.15 to 0.5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
414
MPa    
552 to 689
MPa    
22
% strain    
 
Other Information
As normalized: 70,000-90,000 psi TS; 50,000 YS min; 22 El. Quenched and tempered: 80,000-100,000 psi TS; 60,000 YS min; 22 El. For structural, machinery, and industrial uses to 4 in. thick, weldable.
RQC-60
 