Chemical Composition
0.23
%    
13.4
%    
3.1
%    
71
%    (estimate)
1.2
%    
11.1
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1690 to 1760
MPa    
1930 to 2000
MPa    
14 to 16
% strain    
 
Other Information