Chemical Composition
0.38 to 0.43
%    
0.7
%    
95.5 to 96
%    (estimate)
0.7
%    
0.3
%    
1.5 to 2
%    
0.4
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
689 to 1550
10^7 dyne/cm^2    
827 to 1720
10^7 dyne/cm^2    
3 to 18
% strain    
250 to 500
   
 
Other Information
Normalized: 100,000-130,000 TS; 70,000-95,000 YS; 10-20 El; 25-40 RA; 210-250 HB; Heat treated: 120,000-250,000 TS; 100,000-225,000 YS; 3-18 El; 7-40 RA; 250-500 HB; For machine tool parts, gears, shafts, and castings.