Chemical Composition
0.02
%  (maximum)  
0.08 to 0.13
%    
0.12
%  (maximum)  
0.17
%  (maximum)  
96.2 to 97.4
%    (estimate)
1.63 to 1.87
%    
0.12
%  (maximum)  
0.12
%  (maximum)  
0.02
%  (maximum)  
0.02
%  (maximum)  
0.85 to 1.13
%    
0.07
%  (maximum)  
0.06
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 