Chemical Composition
0.05 to 0.15
%    
31.2 to 46.8
%    (estimate)
20 to 24
%    
3
%  (maximum)  
1.25
%  (maximum)  
20 to 24
%    
0.2 to 0.4
%    
13 to 16
%    
La 0.02-0.12
Co is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
380
MPa    
40
% strain    
 
Other Information
Minimum values at 20 C: 860 N/mm**2 TS; 380 N/mm**2 YS; 40 El. For gas turbines, air heaters, furnace components, high temperature heat exchangers, valves and springs. Material No. 2.4683.
CONICRO 4023 W - ALLOY 188
 