Chemical Composition
0.1
%    
50
%    
20
%    
10
%    
15
%    
 
Mechanical Properties
350
MPa    
35
% strain    
 
Other Information
850 N/mm**2 TS (RT); 350 N/mm**2 YS (RT); 35 El (RT). Corrosion resisting and heat resisting alloy. For parts of gas turbines and transmissions for operation up to 950 C. DIN 2.4964.
SAARSTAHL 2.4964
 



No warranty is given for the accuracy of these data