Chemical Composition
0.05 to 0.15
%    
46.5 to 57
%    (estimate)
19 to 21
%    
3
%  (maximum)  
1 to 2
%    
9 to 11
%    
0.3
%  (maximum)  
14 to 16
%    
Co is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
380
MPa    
30
% strain    
 
Other Information
Minimum values at 20 C: 900 N/mm**2 TS; 380 N/mm**2 YS; 30 El. For gas turbines and furnace components, high temperature equipment, valves and springs. Material No. 2.4964.