Chemical Composition
0.12 to 0.18
%    
0.4
%  (maximum)  
0.3
%  (maximum)  
97.3 to 99.1
%    (estimate)
0.6 to 0.9
%    
0.1
%  (maximum)  
0.4
%  (maximum)  
0.025
%  (maximum)  
0.02 to 0.04
%    
0.15 to 0.4
%    
1) Cast analysis.
2) Steels with improved machinability either by higher S levels up to about 0.10 % S (including controlled sulphide morphology) or Pb additions may be available on request. In the first case, the upper limit of the Mn-content may be increased by 0.15 %.
3) Steels may be supplied with a lower Si content. In this case, alternative means of deoxidation shall be used.
4) Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
DimensionsBrinell Hardness
Thickness, ≥ 5 to ≤ 10 mm≤ 242
Thickness, > 10 to ≤ 16 mm≤ 238
Thickness, > 16 to ≤ 40 mm≤ 222
Thickness, > 40 to ≤ 63 mm≤ 204
Thickness, > 63 to ≤ 100 mm≤ 184

184
 (maximum)  
Soft annealed, cold drawn (+A+C)
 