Chemical Composition
0.025
%  (maximum)  
24 to 26
%    
1.2 to 2
%    
56.8 to 64.3
%    (estimate)
0.8
%  (maximum)  
3 to 4
%    
0.23 to 0.33
%    
6.5 to 8
%    
0.025
%  (maximum)  
0.002
%  (maximum)  
0.8
%  (maximum)  
0.8 to 1.2
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
585
MPa  (minimum)  
820
MPa  (minimum)  
25
% strain  (minimum)  
293
 (maximum)  
 