Chemical Composition
0.28 to 0.34
%    
98.4 to 99
%    (estimate)
0.6 to 0.9
%    
0.04
%  (maximum)  
0.05
%  (maximum)  
0.15 to 0.3
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
340 to 400
MPa    
550 to 650
MPa    
20 to 32
% strain    
163 to 195
   
 