Chemical Composition
0.2 to 0.4
%    
12 to 15
%    
79.5 to 86.3
%    (estimate)
1
%  (maximum)  
1
%  (maximum)  
0.04
%  (maximum)  
0.04
%  (maximum)  
1.5 to 3
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
490
MPa  (minimum)  
 