Chemical Composition
1.1 to 1.3
%    
0.5
%  (maximum)  
84.1 to 87.4
%    (estimate)
11.5 to 13.5
%    
0.06
%  (maximum)  
0.03
%  (maximum)  
0.5
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
345
MPa    
780 to 1080
MPa    
40
% strain    
 
Other Information