Chemical Composition
0.67
%  (maximum)  
0.3
%  (maximum)  
0.3
%  (maximum)  
96.9 to 100
%    (estimate)
0.9
%  (maximum)  
0.08
%  (maximum)  
0.3
%  (maximum)  
0.04
%  (maximum)  
0.04
%  (maximum)  
0.4
%  (maximum)  
0.05
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
Other Information
Links



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®