Chemical Composition
0.28 to 0.35
%    
2.8 to 3.3
%    
94.3 to 96
%    (estimate)
0.4 to 0.7
%    
0.3 to 0.5
%    
0.3
%  (maximum)  
0.03
%  (maximum)  
0.035
%  (maximum)  
0.2 to 0.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
85.6
ksi    
113 to 135
ksi    
14
% strain    
 