Chemical Composition
0.015
%  (maximum)  
0.17 to 0.23
%    
0.3
%  (maximum)  
97.3 to 98.8
%    (estimate)
1 to 1.5
%    
0.035
%  (maximum)  
0.03
%  (maximum)  
0.6
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
Not Applicable
295
MPa    
490 to 590
MPa    
18
% strain    
 