Chemical Composition
0.07
%    
19 to 21
%    
34.9 to 46.9
%    (estimate)
2
%  (maximum)  
2 to 3
%    
32 to 38
%    
1
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
240
MPa    
30
% strain    
 
Other Information