Chemical Composition
0.85
%    
5
%    
92.4
%    (estimate)
0.9
%    
0.55
%    
0.35
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
50 to 55
   
 
Other Information
50-55 HRC; For hard surfacing and build-up for resistance to abrasion and moderate to heavy impact. For dump truck bodies, brake shoe hangers, and bulldozer trunnions. Steel core wire; composite coating.
AIRCO SELF HARDENING
 