Chemical Composition
0.38 to 0.43
%    
0.8 to 1.1
%    
97.3 to 97.9
%    (estimate)
0.75 to 1
%    
0.2
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
634 to 731
MPa    
814 to 910
MPa    
17 to 20
% strain    
235 to 277
   
 
Other Information