Chemical Composition
0.2 to 0.4
%    
93.4 to 96.2
%    (estimate)
0.3 to 0.5
%    
0.3 to 0.7
%    
3 to 5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1450
MPa    
1720
MPa    
8
% strain    
51
   
 
Other Information