Chemical Composition
0.08
%  (maximum)  
12 to 14
%    
61.4 to 69.2
%    (estimate)
17 to 19
%    
0.2 to 0.8
%    
0.1 to 0.35
%    
0.25
%  (maximum)  
1.5 to 3
%    
0.06
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 