Chemical Composition
0.08 to 0.15
%    
0.25 to 0.5
%    
97.7 to 98.6
%    (estimate)
0.4 to 0.7
%    
0.5 to 0.7
%    
0.22 to 0.3
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
291
MPa    
17
% strain    
 