Chemical Composition
1.8 to 2.2
%    
97.8 to 98.2
%    (estimate)
Cu is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
827
MPa    
1100 to 1170
MPa    
2 to 8
% strain    
370 to 400
   
 
Other Information
Heat treated: 160,000-170,000 TS; 120,000 YS; 2-8 El; 4 RA; 370-400 HB; For gears, die molds, rocker arms, non-sparking tools; corrosion resistant, age hardenable.
VICULOY NO. 3
 