Chemical Composition
0.06
%  (maximum)  
15 to 17
%    
2.5 to 4
%    
71.5 to 78.9
%    (estimate)
1
%  (maximum)  
0.15 to 0.4
%    
3.5 to 5
%    
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
965
MPa    
1030
MPa    
9
% strain    
 