E9310, BNCMo3E, MSZ 31 (BNCMo3E, MSZ 31 (0-11 mm))
add data link
Chemical Composition
Base Element
Fe (Iron)
C (Carbon)
0.12 to 0.18
%
Cr (Chromium)
1.1 to 1.4
%
Fe (Iron)
92.8 to 94.3
%
(estimate)
Mn (Manganese)
0.25 to 0.55
%
Mo (Molybdenum)
0.2 to 0.3
%
Ni (Nickel)
3.8 to 4.3
%
P (Phosphorus)
0.035
% (maximum)
S (Sulfur)
0.02 to 0.035
%
Si (Silicon)
0.17 to 0.37
%
Composition Note
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Mechanical Properties
Yield Strength
883
MPa
Ultimate Tensile Strength
1270 to 1620
MPa
Elongation
7
% strain
Other Information
Material Class
Ferrous Alloy
Alloy Family
Alloy Steel
Alloy Group
Nickel chromium molybdenum steel
Alloy Sub-Group
E9310
Country
Hungary
Standards Body
MSZ (Hungary)
Description
Case hardened; 0-11 mm; blank carburized
Designation
BNCMo3E
Specification Type
Standard
Specification
MSZ 31
Specification Year
1974
Specification Status
Active
Source
Worldwide Guide to Equivalent Irons and Steels, 5th ed. ASM International 2006
Available forms
Wrought
Similar Alloys
Click here to find similar alloys
Links
Organizations
Magyar Szabvanyugyi Testulet (MSZT) (Hungarian Standards Institution)
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard