1043, A49, ASTM A49
add data link
Chemical Composition
Base Element
Fe (Iron)
C (Carbon)
0.35 to 0.6
%
Fe (Iron)
98.1 to 99.7
%
(estimate)
Mn (Manganese)
1.2
% (maximum)
P (Phosphorus)
0.04
% (maximum)
S (Sulfur)
0.05
% (maximum)
Composition Note
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Mechanical Properties
Yield Strength
485
MPa (minimum)
Ultimate Tensile Strength
690
MPa (minimum)
Elongation
12
% strain (minimum)
Other Information
Material Class
Ferrous Alloy
Alloy Family
Carbon Steel
Alloy Group
Medium-carbon steel
Alloy Sub-Group
1043
Country
USA
Standards Body
ASTM (USA)
Description
Heat-treated carbon steel joint bars for general use in standard railroad track
Designation
A49
Specification Type
Standard
Specification
ASTM A49
Specification Year
2001
Specification Status
Active
Specification Status Notes
active 2001
Source
Worldwide Guide to Equivalent Irons and Steels, 5th ed. ASM International 2006
Available forms
Wrought
Similar Alloys
Click here to find similar alloys
Links
Organizations
American Society for Testing and Materials (ASTM)
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard