1019, A35K, MSZ 2898/2 (A35K, MSZ 2898/2 (bright-drawn, soft))
add data link
Chemical Composition
Base Element
Fe (Iron)
C (Carbon)
0.17
% (maximum)
Fe (Iron)
97.8 to 99.5
%
(estimate)
Mn (Manganese)
0.4 to 1.6
%
P (Phosphorus)
0.05
% (maximum)
S (Sulfur)
0.05
% (maximum)
Si (Silicon)
0.1 to 0.35
%
Composition Note
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Mechanical Properties
Yield Strength
260
MPa
Ultimate Tensile Strength
370
MPa
Elongation
10
% strain
Other Information
Material Class
Ferrous Alloy
Alloy Family
Carbon Steel
Alloy Group
Low-carbon steel and HSLA steel
Alloy Sub-Group
1019
Country
Hungary
Standards Body
MSZ (Hungary)
Description
Seamless cold formed tube; seamless tubes special requirements; 0.5-10 mm; bright-drawn, soft
Designation
A35K
Specification Type
Standard
Specification
MSZ 2898/2
Specification Year
1980
Specification Status
Active
Source
Worldwide Guide to Equivalent Irons and Steels, 5th ed. ASM International 2006
Available forms
Wrought
Similar Alloys
Click here to find similar alloys
Links
Organizations
Magyar Szabvanyugyi Testulet (MSZT) (Hungarian Standards Institution)
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard