Chemical Composition
0.25
%  (maximum)  
0.5
%    
97.4 to 97.6
%    (estimate)
0.9
%    
0.5
%    
0.5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
345 to 621
MPa    
552 to 827
MPa    
14 to 20
% strain    
150 to 210
   
 
Other Information
Cast: 80,000-120,000 TS; 50,000-90,000 YP; 150-210 HB; 14-20 El. For general and structural applications, gears, shafts, housings. Good weldability. AISI 8620 modified.