Chemical Composition
0.35
%  (maximum)  
0.95
%    
97.7 to 98.1
%    (estimate)
0.8
%    
0.2
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
448 to 689
MPa    
621 to 827
MPa    
14 to 20
% strain    
180 to 260
   
 
Other Information
Cast: 90,000-120,000 TS; 65,000-100,000 YP; 14-20 El; 30-40 RA; 180-260 HB; For general and structural castings, shafts, gears, housings. AISI 413. Shock resistant.