Cast high-copper alloy, NBD UNIVERSAL BABBITT (Abex Corp.)
add data link
Chemical Composition
Base Element
Cu (Copper)
Balance
Cu (Copper)
Other elements
Sn, Pb
Mechanical Properties
Ultimate Tensile Strength
103
MPa
Elongation
1
% strain
Brinell Hardness
40
Other Information
Material Class
Nonferrous Alloy
Alloy Family
Copper
Alloy Group
Cast copper
Alloy Sub-Group
High-copper alloy
Country
USA
Description
Cast: 14,900 TS; 1.0 El; 1.0 RA; 40 HB; For bearings to resist heat; tough Babbitt metal. M. P. 1100 F.
Designation
NBD UNIVERSAL BABBITT
Specification Type
Manufacturer's Specification
Specification Status
Renamed
Source
Woldman's Engineering Alloys 9th ed. J. Frick Editor, ASM International 2000
Available forms
Bearing
,
Casting
Links
Organizations
Abex Corp.
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard