Chemical Composition
0.02
%  (minimum)  
0.2
%  (maximum)  
0.3
%  (maximum)  
0.7
%  (maximum)  
95.2 to 99
%    (estimate)
1 to 1.7
%    
0.1
%  (maximum)  
0.025
%  (maximum)  
0.05
%  (maximum)  
0.8
%  (maximum)  
0.035
%  (maximum)  
0.03
%  (maximum)  
0.6
%  (maximum)  
0.03
%  (maximum)  
0.2
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
Not Applicable
460
MPa  (maximum)  
550 to 720
MPa    
17
% strain  (minimum)  
 
Other Information