Chemical Composition
0.07
%  (maximum)  
0.6 to 0.9
%    
1 to 1.3
%    
95.3 to 97.1
%    (estimate)
0.4 to 0.7
%    
0.15 to 0.25
%    
0.02
%  (minimum)  
0.7 to 1
%    
0.025
%  (maximum)  
0.025
%  (maximum)  
0.4
%  (maximum)  
0.03
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
450
MPa  (minimum)  
515 to 655
MPa    
28
% strain  (minimum)  
197
 (maximum)  
 
Other Information
Links



No warranty is given for the accuracy of these data