Chemical Composition
0.03
%  (maximum)  
21 to 25
%    
45 to 56.2
%    (estimate)
4.5 to 6.5
%    
3 to 3.7
%    
0.3 to 0.5
%    
0.3
%  (maximum)  
15 to 18
%    
1
%  (maximum)  
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
420
MPa    
800 to 1000
MPa    
35
% strain    
 